- Haʻahaʻa haʻahaʻa, ikaika kiʻekiʻe.
- Ka ikaika wela kiʻekiʻe maikaʻi (Reaction bonded).
- Ke kū'ē i ka oxidation (Hoʻopaʻa i ka hopena).
– Kūleʻa haʻalulu wela maikaʻi.
- ʻO ka paʻakikī kiʻekiʻe a me ke kūpaʻa ʻaʻahu.
– Ke kūʻē kemika maikaʻi loa.
- Hoʻonui haʻahaʻa haʻahaʻa a me ka conductivity thermal kiʻekiʻe.
| Nā mea kino | Unite | Waiwai |
| maʻiʻo SIC | % | 95-88 |
| Kuokoa Si | % | 5~12 |
| ʻAno nui | g/cm3 | >3.01 |
| Porosity | % | <0.1 |
| ʻoʻoleʻa | Kg/mm2 | 2400 |
| Coefficient o ka ikaika kulou ma 20 degere Celsius | Mpa | 260 |
| Coefficient o ka ikaika kulou ma 1200 degere Celsius | Mpa | 280 |
| Modulus o ka elasticity ma 20 Degere Celsius | Gpa | 330 |
| ʻOoleʻa haʻihaʻi | Mpa*m1/2 | 3.3 |
| Coefficient o ka thermal conductivity ma 1200 degere Celsius | W/mk | 45 |
| Coefficient o ka hoonui wela ma 1200 degere Celsius | 10-6mm/mmK | 4.5 |
| Coefficient o ka hahana wela | <0.9 | |
| Max.Hana wela | ℃ | <1380 |
| Nānā: ʻO ka ʻikepili o nā waiwai i ʻōlelo ʻia he hopena maʻamau mai nā ʻāpana hoʻāʻo a no laila pono e hoʻohana ʻia ma ke ʻano he alakaʻi | ||